Limp paper (low paper rigidity) is hard to separate from Intermediate Transfer Belt or Paper Transfer Roller.
This is likely to occur if:
The machine runs in high humidity + high temperature, or Low humidity + Low temperature.
Uncoated paper (64 g/m2 or less) or coated paper (100 g/m2 or less) is used.
Short grain paper is used.